Weld to the Wise: Toyota issues repair bulletin on approved welding techniques, cold straightening
Toronto, Ontario — Toyota announced that they are icing the use of heat to straighten body and frame components on OEM repairs, as well as reinforcing pre-existing welding techniques, in a Collision Repair Information Bulletin (CRIB) issued last Wednesday. The automaker says that due to the high-strength sheet steel used for structural body and frame […]